Some unique features of the Endocarb System:
- The Endocarb System is easily programmed using an oxygen probe
- The effective case depth is reached over 30% faster than conventional carburizing
- The Endocarb System uses less than 1/2 of the natural gas of a conventional process
- Unlike conventional carburizing, a very low flow of atmosphere is required
- Very little time is required to establish a 1.45% CP on heat up after shut down
- “Plunge Cooling” – Will cool the load down from carburizing temperature to quench temperature much faster by flowing 100% blower air and 0% gas into the furnace burner
- A sharper drop off in carbon at the effective case depth for a more ductile core
- No endogas from an outside generator is required in the furnace hot zone
- Work loads using this system are always clean
- Atmosphere gas from the endocarb enters the furnace just under 1,825˚F reacted
- Carbon potential will operate from under .40 to 1.45% CP
- Pay back for this system can be less than six months because of shorter cycles
- No catalyst to change as the endocarb unit is self catalytic
- User friendly and very easy to operate
- An unsafe condition will shut down the system and sound an alarm
- Long trouble free life can be expected
- System will operate trouble free with very little maintenance